Yasuda 145-C Hybrid creep tester (Stress relaxation tester)

Model145-C
Warranty1 year
Contact
Secure Checkout
Quality Engagement
Easy change and return
Delivery Available

Hangings: 3, 6 or 10 Hangings, (3 kinds)

Specimen: See JIS-K6263 for reference

Load Method: Pulley Wheel Type or Balance Scale Type

Load Measuring: Load Cell, Max. 500 N (50 kgf)

Displacement Measurement: Magnetic Linear Scale 1/100 mm,Stroke 0 to Max. ± 40 mm(Required confirmation)

Temperature Range: Max. 200 °C

Software: Windows Compatible

Option: Compression Jig, Bending Jig, Low Temperature Oven, Constant Temperature & Humidity Oven, Divided Oven, Gauge Length Measuring Spec

Datasheet


Stay Updated with Offers

Get exclusive volume discounts, bulk pricing updates, and new product alerts delivered directly to your inbox.

By subscribing, you agree to our Terms of Service and Privacy Policy.

Quick Support

Direct access to our certified experts